Welding Heat Input and Preheat Calculator
Enter voltage, current and travel speed to get the heat input, or enter the steel composition, thickness, hydrogen level and heat input to get carbon equivalents and the minimum preheat temperature.
Runs in your browser. Your files never leave your device. See how to check
…
How to do it
- 1Choose the calculation
Heat input or preheat.
- 2Enter the arc data
Volts, amps and travel speed.
- 3Enter the composition
From the mill certificate.
- 4Set thickness and hydrogen
Combined thickness and HD.
- 5Read heat input and preheat
With validity checks.
About this tool
Heat input controls the cooling rate of a weld, and with it the hardness and toughness of the heat-affected zone. EN 1011-1 defines it as Q = k·U·I/v, where k is the thermal efficiency of the process (1.0 for submerged arc, 0.8 for manual metal arc and MIG/MAG, 0.6 for TIG). Hardenable steels also need preheat to avoid hydrogen cracking. The required temperature depends on the steel's carbon equivalent, the thickness, the hydrogen content of the weld metal and the heat input. EN 1011-2 Annex C method B combines them in a formula based on the CET carbon equivalent. This calculator gives heat input, arc energy and total heat, the three common carbon equivalents CE(IIW), CET and Pcm, and the method B preheat temperature with a check on its range of validity.
Who this is for
Welding engineers and coordinators, welding inspectors, fabricators writing WPS documents, and students of welding technology.
Heat input
Q (kJ/mm) = k × U (V) × I (A) × 60 / (1,000 × v (mm/min)) Typical values: 0.5-1.5 kJ/mm for thin sheet MIG, 1-2.5 kJ/mm for structural MAG and MMA, 2-5 kJ/mm for submerged arc. Too low a heat input gives hard, brittle HAZ; too high a heat input lowers toughness and strength in some steels.
Thermal efficiency k (EN 1011-1)
SAW 1.0; MMA, MIG/MAG and FCAW 0.8; TIG and plasma 0.6.
Carbon equivalents
- CE(IIW) = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. Above about 0.45, preheat is usually needed. - CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40, used in EN 1011-2 method B. - Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B, for low-carbon modern steels.
Preheat, EN 1011-2 method B
Tp = 697·CET + 160·tanh(d/35) + 62·HD^0.35 + (53·CET − 32)·Q − 328 °C Valid for CET 0.2-0.5 %, thickness 10-90 mm, hydrogen 1-20 ml/100 g and heat input 0.5-4 kJ/mm. Lower hydrogen consumables (HD ≤ 5) and higher heat input both reduce preheat.
Hydrogen scales
Scale A: more than 15 ml/100 g; B: 10-15; C: 5-10; D: 3-5; E: 3 or less. Basic electrodes baked correctly and solid MIG wires are typically scale D or E.
Worked example
A steel with 0.18 C, 1.4 Mn, 0.1 Cr, 0.02 Mo, 0.1 Ni and 0.15 Cu has CE = 0.46 and CET = 0.34. At 30 mm thickness, HD 5 and 1.5 kJ/mm, the minimum preheat is about 106 °C. MAG welding at 28 V, 250 A and 300 mm/min gives 1.12 kJ/mm.
Interpass temperature
Keep the interpass temperature above the preheat and below the maximum allowed for the steel, often 200-250 °C for structural steels, to protect toughness.
Limits
Method B applies to non-alloy, fine-grain and low-alloy steels within its range. This is not professional engineering advice; follow the qualified WPS.
Worked example
CET 0.34, 30 mm, HD 5, 1.5 kJ/mm: preheat about 106 °C (EN 1011-2 method B).
Quick facts
- Category: Engineering & Construction
- Works in your browser, no sign-up, no upload.
- Your input stays on your device.
- Available in English.
- Content last reviewed:
- Official source: EN 1011-1 heat input Q = k·U·I/v with thermal efficiency factors; carbon equivalents CE(IIW), CET and Pcm; EN 1011-2 Annex C method B preheat formula
Frequently asked questions
How is heat input calculated?
k × voltage × current × 60 / (1,000 × travel speed in mm/min), in kJ/mm.
What is CET?
A carbon equivalent used by EN 1011-2 method B for preheat.
When is preheat needed?
Usually for CE above about 0.45, thick sections and higher hydrogen levels.
Does a higher heat input reduce preheat?
Yes, it slows cooling, but it may reduce toughness.
What hydrogen level should I use?
The consumable's diffusible hydrogen, often 5 ml/100 g or less.
Is my data stored?
No. Welding data you enter stays on this device.