SMT Stencil Aperture Calculator
Avoid insufficient solder on fine-pitch parts by checking that every stencil aperture will release paste cleanly before ordering the stencil.
Runs in your browser. Your files never leave your device. See how to check
…
How to do it
- 1Enter the stencil thickness
In µm.
- 2List the pads
Name and size in mm.
- 3Add a reduction
If you shrink apertures.
- 4Read the ratios
Area and aspect.
- 5Find failures
And the thickest foil allowed.
- 6Choose the stencil
Thinner or stepped if needed.
About this tool
In surface-mount assembly, solder paste is printed through a thin metal stencil. Whether the paste leaves the aperture and lands on the pad, or sticks to the aperture walls, depends on the aperture's size relative to the stencil thickness. Small openings in a thick foil, typical of 0201 passives, fine-pitch QFNs and 0.4 mm pitch BGAs on boards that also carry large connectors, are the usual cause of insufficient solder and open joints. IPC-7525 gives two simple checks. The area ratio, the opening area divided by the area of the aperture walls, should be at least 0.66; the aspect ratio, aperture width divided by stencil thickness, should be at least 1.5. This calculator applies both to a list of pads you enter by name and size, rectangular or round, at any stencil thickness, and marks each pass or fail. It also shows the thickest stencil each aperture can tolerate, which tells you whether a thinner foil or a step stencil is needed, and can apply a percentage reduction per side, as commonly used to reduce paste volume and bridging.
The formulas
- Rectangular aperture: area ratio = L × W / (2 × (L + W) × T). - Round aperture: area ratio = D / (4 × T). - Aspect ratio = smallest aperture dimension / T. Release improves with higher ratios. The 0.66 and 1.5 limits are IPC-7525 guidance for laser-cut stainless steel; electroformed and nano-coated stencils can release well down to about 0.5.
Choosing a thickness
Common foil thicknesses are 100, 120, 125, 130 and 150 µm. Boards with 0.4 mm pitch parts or 0201 passives often use 100 µm, while boards dominated by larger parts use 120 to 150 µm. When a board mixes both, a step stencil, thinner in the fine-pitch areas, solves the conflict.
Reductions
Apertures are often 5 to 10% smaller than the pads for fine-pitch leads to reduce bridging, and window-pane patterns are used on large thermal pads to limit paste volume and voiding. Reductions lower the area ratio, so check again after applying them.
Other influences
Aperture wall smoothness, paste type (type 4 or 5 powder for fine features), squeegee speed and pressure, and board support all affect printing. Solder paste inspection on the first boards confirms the design.
Limits
These are design guidelines, not guarantees; follow your stencil supplier's and assembler's recommendations. The calculator checks geometry only and does not model paste volume or reflow behaviour.
Worked example
At 120 µm, a 0402 pad aperture of 0.6 × 0.5 mm has an area ratio of 1.14 and passes, a 0.5 mm-pitch BGA aperture of 0.3 mm diameter has an area ratio of 0.63 and fails, and the tool shows that this aperture needs a stencil no thicker than about 114 µm.
Quick facts
- Category: Engineering & Construction
- Works in your browser, no sign-up, no upload.
- Your input stays on your device.
- Available in English.
- Content last reviewed:
- Official source: IPC-7525 Stencil Design Guidelines
Frequently asked questions
What area ratio is required?
At least 0.66 under IPC-7525 for standard laser-cut stencils.
What is the aspect ratio?
Aperture width divided by stencil thickness, at least 1.5.
How do I fix failing apertures?
Use a thinner or step stencil, enlarge the aperture, or a better stencil technology.
Which thickness for 0201 parts?
Usually 100 µm or less, or a step stencil.
Do round apertures release better?
They have the same area ratio rule, D / 4T, and are common for BGAs.
Is anything uploaded?
No. Calculations run in your browser.